Impahla | I-solvent free (Isekelwe emanzini) |
Inani lokusabela | ≥ 80% |
Ukumelana nokushelela | 60-80N |
Impahla yokudambisa | 20-35% |
Isivinini saphansi | 30-45 |
Ukujiya okuphelele | 3-4 mm |
Kuhlanganiswe ukusebenzisa isikhathi | <8 amahora (25℃) |
Thinta isikhathi sokumisa | 2h |
Isikhathi sokumisa kanzima | >24 h (25℃) |
Impilo yesevisi | > iminyaka engu-8 |
upende imibala | Umbala we-Mutiple |
Amathuluzi ohlelo | I-roller, i-trowel, i-rake |
Isikhathi sakho | 1 unyaka |
Izwe | Uketshezi |
Isitoreji | I-5-25 degree centigrade, ipholile, yomile |
I-substrate ephekwe ngaphambilini
Isiqalo
Ukugqoka okuphakathi
Ukugqoka okuphezulu
I-varnish (ngokuzikhethela)
IsiceloUbubanzi | |
Isistimu kapende yokunwebeka yaphansi enemisebenzi eminingi nenemisebenzi eminingi yenkundla yezemidlalo yangaphakathi nangaphandle, inkundla yethenisi, inkundla yebasketball, inkundla ye-volleyball, ithrekhi yokugijima, izitshalo zezimboni, isikole, izibhedlela, izindawo zomphakathi, izindawo zokupaka nezakhiwo zomphakathi njll. | |
Iphakheji | |
20kg/umgqomo. | |
Isitoreji | |
Lo mkhiqizo ugcinwe endaweni engaphezu kuka-0 ℃, indawo yokukhipha umoya kahle, enomthunzi nendawo epholile. |
Imibandela Yokwakha
Izimo zokwakha akufanele zibe ngenkathi yomswakama kanye nesimo sezulu esibandayo (izinga lokushisa ≥10℃ futhi umswakama ngu-≤85%).Isikhathi esingezansi sokufaka isicelo sisho izinga lokushisa elijwayelekile ku-25℃.
Isinyathelo Sokufaka Isicelo
Isiqalo:
1. Faka i-hardener ku-primer resin njengo-1:1 (i-primer resin:hardener=1:1 ngesisindo).
2. Hlanganisa zombili izingxenye ndawonye cishe imizuzu engu-3-5 kuze kube yilapho ifana.
3. Faka ingxube ye-primer usebenzisa ibhulashi, i-roller noma isibhamu sokufutha ekugqileni okunconywayo kwama-microns angu-100-150.
4. Vumela i-primer ukuthi ilulame ngokugcwele okungenani amahora angama-24 ngaphambi kokudlulela esinyathelweni esilandelayo.
I-Middle Coating:
1. Faka inhlaka eqinisayo phakathi nendawo njengo-5:1 (inhlaka ephakathi nendawo:i-hardener=5:1 ngesisindo).
2. Hlanganisa zombili izingxenye ndawonye cishe imizuzu engu-3-5 kuze kube yilapho ifana.
3. Faka i-coating ephakathi usebenzisa i-roller noma isibhamu sokufafaza ekugqileni okunconywayo kwama-microns angu-450-600.
4. Vumela ukunamathela okuphakathi ukuthi kwelaphe ngokugcwele okungenani amahora angama-24 ngaphambi kokudlulela esinyathelweni esilandelayo.
I-Top Coating:
1. Faka into eqinisayo kunhlaka enamathelayo ephezulu njengo-5:1 (i-top coating resin:hardener=5:1 ngesisindo).
2. Hlanganisa zombili izingxenye ndawonye cishe imizuzu engu-3-5 kuze kube yilapho ifana.
3. Faka ijazi eliphezulu usebenzisa i-roller noma isibhamu sokufafaza ngobuningi obunconywayo be-100-150 microns.
4. Vumela ukugqoka okuphezulu kuphuluke ngokugcwele okungenani izinsuku ezintathu kuya kweziyisikhombisa ngaphambi kokusebenzisa indawo.
1. Sebenzisa izinto zokuzivikela ezinjengamagilavu, izibuko, kanye nomshini wokuphefumula lapho ubamba upende.
2. Isilinganiso nesikhathi sokuxuba sengxenye ngayinye kufanele ilandelwe ngokuqinile.
3. Faka ungqimba ngalunye ezindaweni ezinomoya omuhle futhi ugweme ukusebenzisa elangeni eliqondile.
4. Ukuhlanza kahle kwendawo kuyadingeka ngaphambi kokusebenzisa i-primer.
5. Ukusebenzisa ngokweqile noma ukusetshenziswa kancane kopende kungase kuholele ezinkingeni ngokuqeda, ngakho landela imihlahlandlela yokuqina enconyiwe.
6. Isikhathi sokuphulukisa sesendlalelo ngasinye singahluka kuye ngokuthi izinga lokushisa kanye nomswakama wendawo, ngakho-ke kungcono ukubheka indawo engaphezulu kuze kube yilapho selapheke ngokugcwele.
Ukufaka upende ophansi wenkundla yezemidlalo we-polyurethane kuyinqubo eqondile edinga ukunakwa kwemininingwane kanye nokuhambisana kahle nemibandela nezinyathelo ezichazwe ngenhla.Indawo eyakhiwe kahle inganikeza ukuqina okuhlala isikhathi eside nokumelana nokuguga.Sithemba ukuthi lo mhlahlandlela unikeza umbono ocacile wenqubo yokufaka isicelo sopende wesitezi senkundla yezemidlalo we-polyurethane, ongasiza ekufinyeleleni umphumela owufunayo wezindawo zakho zemidlalo noma izindawo zemisebenzi eminingi.